Electrode rubber ThermalProperties TemperatureControl LiquidCrystal ForceVolumeImage Pinpoint Mechanical&nanotechnology hard_disk_media NCM\ NUS_Physics HDD Reading PiezoelectricForceMicroscopy CNT fluoroaalkane Spain Piezoelectric SiliconCrystal CeNSE_IISc Polypropylene food solar_cell HiVacuum Polytetrafluoroethylene ito_film Defects Implant BreastCancerCell Zhi AdhesionForce Hexylthiophene Gallium_Arsenide ForceVolumeMapping LiquidImaging
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Plate-shaped DNA origami
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 1Hz
- Scan Size : 250nm×250nm
- Pixel Size : 512×256
- Cantilever : USC-F0.3-k0.3 (k=0.3N/m, f=300kHz)