AdhesionEnergy Polarization Roughness ReflexLens Force-distance Biology Steps vertical_PFM ULCA MultiferroicMaterials Phase ScanningThermalMicroscopy Mechinical ScratchMode PvdfBead Ferrite DeflectionOptics PolycrystallineFerroelectricBCZT NTU ElectroDeposition PolyStylene University_of_Regensburg semifluorinated alkane LateralPFM kelvin probe force microscopy MembraneFilter SiliconOxide PvdfFilm tip_bias_mode Wildtype MagneticArray SiWafer Nanofiber Moire Cell
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block Copolymer Embedded in Rubber
Block copolymer embedded in rubber cross-section.
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.29Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.29Hz
- Pixel Size: 256 × 256