Self-assembledMonolayer Gold ScanningThermalMicroscopy Vortex PolycrystallineFerroelectricBCZT Heating contact SiliconeOxide Galfenol Alkane temp IndiumTinOxide Polyethylene AtomicLayer Anneal CancerCell Conducting Genetic ElectroChemical Praseodymium Alloy Fluoride DNAProtein Nanopattern dielectric_trench KevlarFiber ForceDistanceSpectroscopy Oxidation HanyangUniv Glass Hydroxyapatite IcelandSpar Sio2 PhaseTransition HardDiskMedia
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256