Ni81Fe19 Galfenol Hydroxyapatite Plug ScanningThermalMicroscopy tip_bias_mode DataStorage contact Non-ContactMode HexacontaneFilm medical ChemicalCompound Sidewall ForceVolumeImage Gallium_Arsenide light_emission Typhimurium ForceDistanceSpectroscopy AEAPDES mechanical_property Tungsten_disulfide silicon_oxide BloodCell MolecularSelfAssembly PolyimideFilm CopperFoil ContactModeDot Phenanthrene Battery Regensburg ImideMonomer Croatia semifluorinated_alkanes Wonseok Fujian
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256