Conductivity doped Graphite Ram Permalloy atomic_steps Optoelectonics cooling thermal_conductivity Hole PpLdpe Defects VinylAlcohol TCS Techcomp UnivOfMaryland Heat plastics Wonseok BreastCancerCell Metal-organicComplex NusEce ConductiveAFM Tapping Ca10(PO4)6(OH)2 Dimethicone Magnets blended polymers CancerCell Morphology NUS_NNI_Nanocore PhaseImaging Glass Holes Chloroform
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/PVAc Film
Film of Polystyrene/poly(vinyl acetate) blend on Si
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256