PrCurve LiftHeight hydrocarbon FailureAnalysis margarine Neodymium temp_control Singapore UnivMaryland Indent Sulfur Treatment CalciumHydroxide layers SRAM Adhesion SoftSample dielectric_trench molecular_self_assembly PolyimideFilm Au111 cross section Granada ferromagnetic LeakageCurrent BismuthVanadate conductive Change Polyurethane Graphene ConductiveAFM KAIST Melt ScanningTunnelingMicroscopy BloodCell
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512