LeakageCurrent temperature controller AFM CP-AFM TPU AEAPDES mono_layer MultiferroicMaterials Celebration Bacterium NCM Multiferroic_materials NeodymiumMagnets Cobalt-dopedIronOxide Oxidation Austenite Hair Lanthanum_aluminate Silicon EFM Tin sulfide Flake Hydroxyapatite sputter IcelandSpar Semiconductor Ptfe Polyvinylidene HanyangUniv semifluorinated_alkane Sidewall HfO2 Cancer Mosfet Phase molecular_self_assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Kevlar fiber
Scanning Conditions
- System: XE7
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256