Vortex FFM I-VSpectroscopy Non-ContactMode Aggregated_molecules PhaseImaging PyroelectricDetector CeramicCapacitor Tungsten ElectroChemical GlassTemperature NUSNNI Phase HexagonalBN ForceVolume Techcomp hard_disk DNA graphene_hybrid KevlarFiber PatternedSapphireSubstrat fluoroalkane heterojunctions Hexylthiophene electrospinning molecules Topography phase_change Biofilm SrO IcelandSpar LiIonBattery InorganicCompound Ca10(PO4)6(OH)2 Strontium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer thin film
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512