LogAmplifier Indium_tin_oxide NtuEee Spincast Chungnam_National_University CrossSection ItoGlass TungstenDeposition LithiumNiobate PetruPoni_Institute CalciumHydroxide TipBiasMode Kevlar DentalProsthesis CBD MultiLayerCeramicCapacitor MolybdenumDisulfide Laser Inorganic_Compound StrontiumTitanate PANI Stiffness fe_nd_b Cobalt-dopedIronOxide TemperatureControllerStage 2d_materials Writing MagneticPhase domain_switching UnivOfMaryland HexagonalBoronNitride Polarization Gold semifluorinated_alkane Temperature
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512