Crystal Aluminum MLCC ForceMapping Vacuum FailureAnlaysis Modulus Platinum neodymium_magnets hydrocarbon SingleLayer LightEmiting PetruPoni_Institute Ptfe BaTiO3 Zhi DIWafer PolymerPatterns MonoLayer LogAmplifier cannabidiol ForceVolume Forevision Deposition DataStorage OpticalElement Ni81Fe19 HexagonalBoronNitride Polarization Piranha molecules PatternedSapphireSubstrat Phase PUR Polytetrafluoroethylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 4096×2048