ElectrostaticForceMicroscopy NCM Polyvinylidene_fluoride Styrene OpticalWaveguide Tape Global_Comm HiVacuum PANI Titanate PVAC Film CHRYSALIS_INC TemperatureControllerStage temperature_control Regensburg domain_switching Crystal Reduction MBE HexagonalBN Chemical Vapor Deposition Electrical&Electronics BiFeO3 Scanning_Thermal_Microscopy LDPE Ceramics FM_SKPM IVSpectroscopy WWafer ContactModeDots Oxide KPFM StyreneBeads SmalScan
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
STO(SrTiO3), Annealed LAO(LaAlO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm, 5μm×5μm
- Scan Rate: 0.8Hz, .9Hz
- Pixel: 512×512, 256×256