semifluorinated_alkane AtomicSteps Hafnia Inorganic AM-KPFM Heating FM_KPFM Electronics StyreneBeads Domain AEAPDES Scratch cannabidiol MfmPhase KevlarFiber MetalCompound Fet SelfAssembly ElectrostaticForceMicroscopy Nanofiber SiWafer INSPParis AtomicLayer Blend Polymer BloodCell PolyimideFilm Platinum PatternedSapphireSubstrat LightEmission AAO Strontium ForceVolumeMapping Ceramics solar_cell
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)