ForceVolumeMapping MolybdenumDisulfide Polystyrene PtfeMembrane Sphere fifber Conductance EFMAmplitude BloodCell OpticalModulator ScanningTunnelingMicroscopy TungstenThinFilmDeposition CrossSection STM CuParticle Global_Comm Lanthanum_aluminate Polypropylene plastics self_healing Cross-section bias_mode AtomicSteps Step LiBattery FrequencyModulation sputter Polymer temperature controller AFM GalliumPhosphide SurfaceOxidation DNAProtein Tungsten Optical Inorganic_Compound
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric superlattices in 2L-hBN (0°)
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.3 Hz
- Scan Size : 3μm×3μm, 4μm×4μm
- Pixel Size : All 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)