fluoroaalkane Cobalt-dopedIronOxide NUS_NNI_Nanocore Imprint PyroelectricDetector align Current ElectrostaticForceMicroscopy CeNSE_IISc Topography solar_cell PiezoelectricForceMicroscopy PolyStylene Calcium Steps SrO NusEce PinpointNanomechanicalMode Regensburg India ContactModeDot block_copolymer Carbon TipBiasMode Ram Formamidinium_lead_iodide LightEmiting F14H20 Biofilm DNAProtein LiquidImaging Metal PatternedSapphireSubstrat Grain Temasek_Lab
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian