WWafer graphene_hybrid PVAC ScanningTunnelingMicroscopy PtfeFilter SKPM Etch Lattice Ferroelectric CopperFoil Wang Growing Tungsten_disulfide Nanostructure Chromium Vac Polymer medical Device SmalScan DOE Hafnia GlassTemp IndiumTinOxide Conductance InLiquid Multiferroic_materials semifluorinated alkane EvatecAG PhthalocyaninePraseodymium SmallScan AEAPDES CrAu Writing AdhesionEnergy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256