India MagneticForce Global_Comm Modulus CuParticle Growth CancerCell Tungsten_disulfide Tapping YttriaStabilizedZirconia Multiferroic_materials Materials Al2O3 HanyangUniv biocompatible MeltingPoint CuSubstrate amplitude_modulation InLiquid VerticalPFM Cobalt FastScan #Materials LeakageCurrent multi_layer Glass MolecularSelfAssembly Carbon PinPointMode WS2 gallium_nitride Dr.JurekSadowski Celebration Aluminum StainlessSteel
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz