TemperatureControllerStage Collagen Pores Wonseok TCS FloppyDisk PMNPT Sphere BreastCancerCell Laser Leakage Vinylpyridine China self_assembly PS_PVAC Hysteresys Litho Nanotechnology Fujian PtfeMembrane GlassTemperature FM-KPFM Perovskite atomic_steps Yeditepe SiWafer PANI biocompatible organic_polymer Singapore Subhajjit DeoxyribonucleicAcid Pipette Non-ContactMode Sio2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B Alloy
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm