ScanningSpreadingResistanceMicroscopy ConductiveAFM Friction MembraneFilter Photovoltaics LiIonBattery SingleLayer Metal-organicComplex Change atomic_steps FuelCell mono_layer Optoelectonics CrossSection OpticalWaveguide Worcester_Polytechnic_Institute Step Perovskite FM-KPFM Conductive AFM EFMAmplitude MetalCompound Permalloy Alloy heterojunctions BiVO4 ForceVolume SAM ScratchMode Adhesion Self-assembledMonolayer Film Phenanthrene NtuEee Wafer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cannabidiol(CBD) Molecules
CBD(concentration: 20 mg/mL) molecules assembled on Mica surface after solution rinsing Aggregated CBD molecules as a ring shape.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256