Phenanthrene doped MolecularSelfAssembly fluoroalkane KPFM Chemical_Vapor_Deposition Strontium IVSpectroscopy Piezoresponse Trench GaP Hexylthiophene Melt C60H122 HighAcpectRatio AdhesionForce Lateral Mapping SRAM TungstenDeposition Copolymer MfmPhase nanomechanical Silver HfO2 PolyvinylAcetate Semiconductor block_copolymer Styrene DeoxyribonucleicAcid ElectroDeposition AdhesionEnergy fe_nd_b cannabinoid PtfeFilter
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BFO (BiFeO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 5μm×5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512