piezoelectric force microscopy plastics 2d_materials ForceVolume HighAspect MoirePattern Sapphire self-assembly rubber Oxidation Boundary MfmAmplitude margarine SrTiO3 Treatment PS_PVAC AAO Nickel Reading suspended_graphene non_contact HighResolution Organic PolyvinylAcetate thermoplastic_elastomers Defect Foil Wildtype LiIonBattery Laser LiftHeight DiffractiveOpticalElements Molybdenum_disulfide Device cross section
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric superlattices in 2L-hBN (0°)
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.3 Hz
- Scan Size : 3μm×3μm, 4μm×4μm
- Pixel Size : All 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)