food ItoGlass Carbon Nanostructure Jason BTO temperature controller AFM mfm_amplitude Reduction Singapore Spain NTU ThermalConductivity LMF SicMosfet SurfaceChange PVAP3HT 2dMaterials ContactMode Aggregated_molecules CrAu University_of_Regensburg Tin disulfide suspended_graphene Pvdf hard_disk_media conductive PyroelectricDetector PFM MfmAmplitude TemperatureControlledAFM TyphimuriumBiofilm Fe_film Nickel Sapphire
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fractals of silver nanoparticles
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.31 Hz, 0.27 Hz
- Scan Size : 50μm2, 40μm2
- Pixel Size : All 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)