Regensburg Conduct Optic DIWafer LowDensityPolyethylene SSRM Pattern Metal-organicComplex KAIST hetero_structure HexagonalBN PDMS CrystalGrowing MagneticArray Anneal Yeditepe_University Reduction Pore frequency_modulation Led Lift FAPbI3 LiNbO3 exfoliate LightEmission Nanopattern EPFL temp GaN biocompatible Polyvinylidene vertical_PFM LifeScience Gong EFMAmplitude
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
TPU Plastic Thin Film
Thermoplastic polyurethane (TPU) is polyurethane plastics with many properties, including elasticity, transparency, and resistance to oil, grease and abrasion.
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint
- Cantilever: PPP-CONTSCR (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.28Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint
- Cantilever: PPP-CONTSCR (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.28Hz