UnivOfMaryland AtomicLayer EvatecAG Phenanthrene MagneticArray fifber MLCC PinpointNanomechanicalMode ReflexLens AM-KPFM CastIron pinpoint mode LightEmiting chemical_compound thermal_property Liquid WS2 temperature_control membrane Annealing Christmas HexagonalBoronNitride Electrode small_scan PolymerPatterns PpLdpe Thermal LiquidImaging NUSNNI ElectrostaticForceMicroscopy Friction PtfeFilter Calcite CaMnO3 PhthalocyaninePraseodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System: NX20
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256