MESA structure Plug medical Mechanical&nanotechnology multi_layer semifluorinated alkane Mechanical self_assembly Gallium_Arsenide Granada LiquidCrystal Tape TemperatureControlledAFM Nanopattern HighAspect ElectroDeposition I-VSpectroscopy Steps CeramicCapacitor Modulus SmalScan PolyvinylAcetate Bismuth LogAmplifier Pinpoint PFM HighResolution Non-ContactMode ThermalProperties aluminum_nitride SingleLayer SingleCrystal doped InorganicCompound polymeric_arrays CrossSection
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Supramolecular Polymer
Self-folding of supramolecular polymers.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512