CopperFoil Vacuum ScanningTunnelingMicroscopy Forevision oxide_layer Ito AM_SKPM MonoLayer ContactModeDot HOPG SSRM TiO2 Chungnam_National_University ContactModeDots sputter Insulator Dopped H-BN PtfeMembrane Alkane LMF Gallium 2dMaterials DLaTGS 2-vinylpyridine nanomechanical PyroelectricDetector KPFM TemperatureControllerStage lift_mode HiVacuum IMT_Bucharest PolyimideFilm Floppy block_copolymer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256