University_of_Regensburg DIWafer Ucl Thermal FailureAnalysis suspended_graphene temp oxide_layer PrCurve Carbon FastScan MagneticPhase Beads Scratch fluoroalkane Austenite SiliconeOxide LogAmplifier RedBloodCell PolymerPatterns SrO DataStorage light_emitting Pinpoint PFM Chemical_Vapor_Deposition nanobar Granada chemical_compound ULCA 2dMaterials optoelectronics mechanical property FFM IRDetector Phosphide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer thin film
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512