AdhesionEnergy 2dMaterials ScanningThermalMicroscopy Yeditepe_University Molybdenum electrospinning self_healing temp Solar Patterns PMNPT Korea Gallium I-VSpectroscopy UnivOfMaryland Optoelectronic BiFeO3 Defect BlockCopolymer CompactDisk ThermalDetectors MESA structure Temasek_Lab optoelectronics CopperFoil Metal-organicComplex CBD INSPParis Polystyrene Water 2-vinylpyridine TipBiasMode INSP CancerCell ferromagnetic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512