Gallium_Arsenide strontiu_titanate Nickel MechanicalProperty UnivMaryland Chrome Bio NtuEee VinylAlcohol PetruPoni_Institute EFMAmplitude Force-distance Co/Cr/Pt Growth LiquidCell electrospinning 3-hexylthiophene Tungsten LowDensityPolyethylene non_contact LMF Switching Magnetic Force Microscopy TCS Magnetostrictive Optoelectronic SoftSample self_assembly Hole RedBloodCell Phase Display KevlarFiber Lateral_Force_Microscopy LightEmiting
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V