dielectric trench PatternedSapphireSubstrat CaMnO3 MechanicalProperties DNAProtein Kevlar neodymium_magnets DentalProsthesis MetalCompound BismuthFerrite SiliconOxide Pzt ThermalConductivity OrganicSemiconductor Granada Co/Cr/Pt FastScan PECurve SrTiO3 AdhesionEnergy Singapore polymeric_arrays temperature controller AFM silicon_oxide Stiffness CarbonNanotube Array WPlug DIWafer Filter FrictionalForceMicroscopy Hexylthiophene Resistance TyphimuriumBiofilm PhthalocyaninePraseodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PZT thin film
Scanning Conditions
- System: NX10
- Scan Mode: PFM (DC-EFM)
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512