Hole plastics rubber AIN Scratch Etch Foil Korea oxide_layer AM_KPFM TungstenThinFilmDeposition food AdhesionEnergy ForceDistanceSpectroscopy Self-assembledMonolayer CBD Piezo Bmp Polyethylene Pore CHRYSALIS_INC Terrace PANI ContactModeDots polymeric_arrays GlassTemperature Defects vertical_PFM self_healing Semiconductor InorganicCompound Copper small_scan PUR IcelandSpar
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024