BTO MolybdenumDisulfide LiBattery CalciumHydroxide Nanofiber Copolymer graphene_hybrid Kevlar atomic_layer polymeric_arrays Ferrite CancerCell PS_LDPE Pore Conductance LaAlO3 CeramicCapacitor ElectrostaticForceMicroscopy hetero_structure AEAPDES LeakageCurrent ferromagnetic C36H74 Mapping CompactDisk TCS OpticalWaveguide MembraneFilter MagneticPhase DIWafer hydrocarbon Electronics atomic_steps Subhajjit Granada
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li stripping-plating on Li surface
Scanning Conditions
- System : NX10 in dry room
- Scan Mode: Contact/EC AFM
- Scan Rate : 0.15 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : Multi75-G
- ECr : Li metal (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)
- Open circuit voltage : 1 VLi/Li+