IVSpectroscopy InorganicCompound Polyethylene Gallium_Arsenide Led multi_layer Conduct TPU mono_layer C_AFM HighResolution AM-KPFM Device MagneticForceMicroscopy Fiber AtomicLayer Adhesion PolyvinylAcetate Ceramics DomainSwitching Fet P3HT hard_disk_media CeNSE_IISc thermal_conductivity Pore SKKU Writing PVAC KevlarFiber PANI thermoplastic_elastomers CHRYSALIS_INC LateralPFM self_assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)