2dMaterials Nanostructure norganic Tin disulfide hard_disk semifluorinated_alkane temperature controller AFM LFM Led NUSNNI Pore GranadaUniv Yeditepe CaMnO3 IMT_Bucharest TungstenThinFilmDeposition Reading CuSubstrate InorganicCompound Battery Current Strontium SurfaceChange Boron ConductingPolymer PtfeMembrane cooling Thermoplastic_polyurethane IIT-chennai MfmAmplitude Glass Barium_titanate temperature_control OpticalElement BiFeO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
hBN-few layer Graphene
Scanning Conditions
- System : NX10
- Sample bias: 1.75 V
- Scan Mode: C-AFM
- Scan Rate : ALL 0.5Hz
- Scan Size : 200nm×200nm
- Pixel Size : 2048×2048
- Cantilever : AD-2.8-AS (k=2.8N/m, f=75kHz)