LogAmplifier Wang Ptfe Hexylthiophene solar_cell Photovoltaics Christmas FM_KPFM Sadowski Jason Singapore Modulus ReflexLens Gold Polypropylene Phase MoirePattern HexagonalBN MechanicalProperties PolyvinylAcetate align Patterns Varistor Polydimethylsiloxane TPU Treatment ConductingPolymer self-assembly Mechanical&nanotechnology Polarization ULCA ForceMapping Chloroform LiquidCell SiliconCrystal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Crosslinked starch & pectin fibers
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Tapping
- Scan Rate : 0.31 Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : ContSCR (k=0.2N/m, f=25kHz)