LiftHeight doped CHRYSALIS_INC Resistance BismuthFerrite TriGlycineSulphate StrontiumTitanate NtuEee Pyroelectric Layer Pzt FAPbI3 Domain Semiconductor HighAcpectRatio MechanicalProperty mechanical property Reduction Topography Composition rubber Cross-section Hafnia fluoroaalkane Display Molybdenum ScanningIon-ConductanceMicroscopy Inorganic light_emission Pipette Sulfur GranadaUniv fluoroalkane AM-KPFM Battery
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Moire pattern of MoS₂-WSe₂
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 3Hz
- Scan Size : 500nm×500nm
- Pixel Size : 512×512
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)