PetruPoni PinPointMode CarbonNanotube Styrene Silicon ForceVolumeImage Flake medical Adhesion PiezoelectricForceMicroscopy aluminum_nitride Singapore CHRYSALIS_INC graphene_hybrid Litho Ptfe FailureAnalysis Tape PatternedSapphireSubstrat PolyvinylAcetate FuelCell mechanical property #Materials Laser Indent Lateral AdhesionForce Bismuth Sulfur Pores GranadaUniv NUS plastic Carbon HighAcpectRatio
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)