Temasek_Lab Indent Forevision Foil Insulator Heating Anneal Aluminum YszSubstrate HfO2 ferromagnetic FrequencyModulation DeflectionOptics PVAC alkanes margarine Piezoelectric Genetic Lateral_Force_Microscopy DLaTGS Hysteresys FloppyDisk Tapping Adhesive Aggregated_molecules Solution AtomicLayer ScratchMode Battery Zagreb PinPointMode Vac Platinum GlassTemp Al2O3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Star of Graphene
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 0.6 Hz
- Scan Size : 2.5μm×2.5μm
- Pixel Size : 256×256
- Cantilever : Multi75-G (k=3N/m, f=75kHz)