2dMaterials Al2O3 LateralForceMicroscopy PMNPT high_resolution EvatecAG biocompatible Tape Yeditepe_University PolycrystallineFerroelectricBCZT atomic_steps Praseodymium Yeditepe Electrode H-BN Copolymer Hole GalliumPhosphide FloppyDisk Temasek_Lab CBD TemperatureControlledAFM HexacontaneFilm gallium_nitride TemperatureControllerAFM GaP GaAs MechanicalProperties MfmAmplitude Hexatriacontane Layer IndiumTinOxide BTO CastIron ItoGlass
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Christmas Ball Lithography on Si
Create oxidation layers on bare Si surface using bias mode of lithography.
Scanning Conditions
- System: NX10
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area