HexagonalBoronNitride IISCBangalore Multiferroic_materials PolycrystallineFerroelectricBCZT Ito Platinum Subhajjit University_of_Regensburg MetalCompound Materials Piranha SKPM Boundary MolecularSelfAssembly ito_film HfO2 Alloy Tape FrictionalForceMicroscopy Reading CastIron cooling Protein graphene_hybrid Aluminium_Oxide NUS_NNI_Nanocore Lift ScratchMode piezoelectric force microscopy Fluoride Sidewall HardDisk DiffractiveOpticalElements LiNbO3 Sphere
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF Fibrous Membrane
PVDF fibrous membrane made by electrospinning.
Scanning Conditions
- System: NX10
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256