SrTiO3 Adhesive ScanningThermalMicroscopy FM_SKPM Non-ContactMode DLaTGS mfm_amplitude Hafnium_dioxide ElectroDeposition thermal_conductivity 3-hexylthiophene Phthalocyanine Layer Wang AdhesionEnergy DeoxyribonucleicAcid Liquid Electrode Glass PolymerBlend GalliumPhosphide bias_mode Scanning_Thermal_Microscopy ScratchMode SRAM Water SurfaceChange IISCBangalore ThermalConductivity strontiu_titanate mono_layer ContactModeDot FuelCell Defects Indium_tin_oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferromagnetic Nanobars Array
Ferromagnetic nanobars arranged on a Penrose P2 tiling. The Permalloy (Ni81Fe19) nanobars are 810 nm and 500 nm long. The width and thickness of a nanobar amount to about 120 nm and 25 nm, respectively.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm