MechanicalProperties Hole TiO2 TPU Ca10(PO4)6(OH)2 Spain thermoplastic_elastomers Implant TriGlycineSulphate SurfaceOxidation CP-AFM PetruPoni_Institute temperature_control LowDensityPolyethylene Moire ContactMode TemperatureControlledAFM IRDetector Indent BoronNitride SiliconOxide MetalCompound CrystalGrowing self_healing Sperm HighAspect TungstenDeposition Composite Bismuth DLaTGS piezoelectric force microscopy MfmPhase Gallium DNA plastics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe Thin Films
MFM images of Fe thin films (80 nm) epitaxied on GaAs(001) and then implanted with N-atoms. Images reveal weak stripe domains at magnetic remanence.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm