FAPbI3 Topography Nickel MolecularSelfAssembly solar_cell silicon_carbide Ito LiquidCrystal HafniumDioxide Lattice Chromium PetruPoni C60H122 SiliconOxide IRDetector TyphimuriumBiofilm SThM Terrace temperature controller AFM PvdfFilm dichalcogenide molecules Potential IcelandSpar rubber Deposition Nanopattern Logo FM-KPFM Metal-organicComplex MeltingPoint SmallScan Wonseok silicon_oxide Scratch
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Supramolecular Polymer
Self-folding of supramolecular polymers.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512