Worcester_Polytechnic_Institute ThermalProperties PinpointNanomechanicalMode IMT_Bucharest thermoplastic_elastomers Nanofiber ULCA CeramicCapacitor HardDiskMedia SRAM Ni81Fe19 Hole Fendb Chungnam_National_University Materials SmalScan AmplitudeModulation FloppyDisk GranadaUniv Electronics temperature controller AFM Implant ChemicalCompound ForceVolumeImage INSP frequency_modulation mechanical_property semifluorinated alkane Wang Metal-organicComplex Bacteria Topography UnivMaryland LMF Conduct
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Carbon Nanotube on Si
Scanning Conditions
- System: XE7
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128