ScanningTunnelingMicroscopy Pinpoint LFM mono_layer Modulus Vanadate PolyvinylideneFluoride Self-assembledMonolayer Crystal phase_change LowDensityPolyethylene TemperatureControl contact strontiu_titanate Foil Chemical_Vapor_Deposition TappingMode BoronNitride F14H20 Phenanthrene Celebration PS_PVAC organic_polymer plastics NanoLithography Tungsten_disulfide dichalcogenide DataStorage Bacterium AdhesionForce Polymer StainlessSteel LiNbO3 Molybdenum WS2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512