CVD ThermalConductivity PolycrystallineFerroelectricBCZT Sadowski Platinum dielectric trench TyphimuriumBiofilm ForceVolumeImage Metal thermal_conductivity TipBiasMode Sphere Cell temperature controller AFM Hysteresys StyreneBeads Graphite Pattern TransitionMetal cannabinoid Co/Cr/Pt high_resolution Wang LiNbO3 Ram Dopped domain_switching Yttria_stabilized_Zirconia Biofilm TungstenThinFilmDeposition epitaxy INSP InsulatorFilm GlassTemperature LowDensityPolyethylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
SnS2 Flakes
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC240TS (k=2N/m, f=70kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC240TS (k=2N/m, f=70kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256